• TA6V ELI
  • Titane TA6V ELI

  • Grade 23

Norms AMS 4907, AMS 4930, AMS 4956, ASTM B-337, ASTM F 136-92, ISO 5832

Production technique Drawn, Rolled

Chemical composition Mechanical characteristics
Al Fe Ti V Other Rm Rp A% HB Density W/m.k
IACS
5,5-6,5 ≤ 0,25 Reste 3,5-4,5 ≤ 0,273 ≥ 980 ≥ 900 ≥ 17 315 4,43 7,3
Description

The ELA (Extra Low Intersticials) grade of TA6V was developed to improve toughness and ductility at very low temperatures. Biocompatible. Recommended in seawater under stress. Fairly good weldability. Forging ability.

Application

Engine and structural parts with strong toughness. Surgical Implants.